Transmitted Data
| Use these instructions for keypad installations only. If a computer will be attached to the module, skip this section. All setup functions will be done in the analysis software application. |
Analysis and calibration data can be transmitted in a single column or spreadsheet with data in ASCII delimited format. Units are displayed as:
| Type | Measurement |
|---|---|
| Date | DD/MM/YY |
| Time | HH:MM:SS |
| Pressure | psig |
| Temperature | °C |
| Elapsed Time | seconds |
Analysis Report
| Record Number |
Description | Form |
|---|---|---|
| 1 | Version Number | 20 characters |
| 2 | Serial Number | 1 integer |
| 3 | Report type = analysis | 8 characters |
| 4 |
Start (reported on one line as ASCII comma delimited data)
|
8 characters (each) |
| 5 |
Stop (reported on one line as ASCII comma delimited data)
|
8 characters (each) |
| 6 | Temperature | 1 floating point |
| 7 | Description line 1 | 20 characters |
| 8 | Description line 2 | 20 characters |
| 9 | Sample IDs | 20 characters |
| 10 | Sample mass | 1 floating point |
| 11 | Number of purges | 1 integer |
| 12 | Equilibration rate | 1 floating point |
| 13 |
Chamber Insert:
1 cm3 (10 cm3 unit) 0.1 cm3 (1 cm3 unit)
3.5 cm3 (10 cm3 unit) |
1 integer |
| 14 | Cell volume | 1 floating point |
| 15 | Expansion volume | 1 floating point |
| 16 | Average volume | 1 floating point |
| 17 | Volume standard deviation | 1 floating point |
| 18 | Average density | 1 floating point |
| 19 | Density standard deviation | 1 floating point |
| 20 | Number of runs | 1 integer |
| 21 |
Run precision
|
1 floating point |
| 22 | Percent full scale | 1 floating point |
| 23 | Carriage return / Line feed | |
| 24 | Carriage return / Line feed | |
| 25 | Carriage return / Line feed | |
| 26 | Run number and pressure (reported on one line as ASCII comma delimited data) | |
| 26a |
Run number |
1 integer |
| 26b |
P1 |
1 floating point |
| 26c |
P2 |
1 floating point |
| 26d |
Include in average calculation
|
1 integer |
| 26e |
Elapsed time |
1 unsigned integer |
| 26f |
Volume |
1 floating point |
| 26g |
Volume deviation |
1 floating point |
| 26h |
Density |
1 floating point |
| 26i |
Density deviation |
1 floating point |
| 27 | Temperature (all temperature data) | 1 floating point |
Calibration Report
| Record Number |
Description | Form |
|---|---|---|
| 1 | Version Number | 20 characters |
| 2 | Serial Number | 1 integer |
| 3 | Report type = calibration | 11 characters |
| 4 |
Start (reported on one line as ASCII comma delimited data)
|
8 characters (each) |
| 5 |
Stop (reported on one line as ASCII comma delimited data)
|
8 characters (each) |
| 6 | Temperature | 1 floating point |
| 7 | Calibration standard size | 1 floating point |
| 8 | Number of purges | 1 integer |
| 9 | Equilibration rates | 1 floating point |
| 10 |
Chamber Insert:
1 cm3 (10 cm3 unit) 0.1 cm3 (1 cm3 unit)
3.5 cm3 (10 cm3 unit) |
1 integer |
| 11 | Average cell volume | 1 floating point |
| 12 | Cell volume standard deviation | 1 floating point |
| 13 | Average expansion volume | 1 floating point |
| 14 | Expansion volume standard deviation | 1 floating point |
| 15 | Number of runs | 1 integer |
| 16 | P1 (all P1 data) | 1 floating point |
| 17 | P2 (all P2 data) | 1 floating point |
| 18 | P1* (all P1* data) | 1 floating point |
| 19 | P2* (all P2* data) | 1 floating point |
| 20 |
Include in average calculation
|
1 integer |
| Record Number |
Description | Form |
|---|---|---|
| 1 | Version Number | 20 characters |
| 2 | Serial Number | 1 integer |
| 3 | Report type = calibration | 11 characters |
| 4 |
Start (reported on one line as ASCII comma delimited data)
|
8 characters (each) |
| 5 |
Stop (reported on one line as ASCII comma delimited data)
|
8 characters (each) |
| 6 | Temperature | 1 floating point |
| 7 | Calibration standard size | 1 floating point |
| 8 | Number of purges | 1 integer |
| 9 | Equilibration rates | 1 floating point |
| 10 |
Chamber Insert:
1 cm3 (10 cm3 unit) 0.1 cm3 (1 cm3 unit)
3.5 cm3 (10 cm3 unit) |
1 integer |
| 11 | Average cell volume | 1 floating point |
| 12 | Cell volume standard deviation | 1 floating point |
| 13 | Average expansion volume | 1 floating point |
| 14 | Expansion volume standard deviation | 1 floating point |
| 15 | Number of runs | 1 integer |
| 16 | Carriage return / Line feed | |
| 17 | Carriage return / Line feed | |
| 18 | Carriage return / Line feed | |
| 19 | Run number and pressure (reported on one line as ASCII comma delimited data) | |
| 19a |
Run number |
1 integer |
| 19b |
P1 |
1 floating point |
| 19c |
P2 |
1 floating point |
| 19d |
P1* |
1 floating point |
| 19e |
P2* |
1 floating point |
| 19f |
Include in average calculation
|
1 integer |
| 19g |
Cell volume |
1 floating point |
| 19h |
Cell volume deviation |
1 floating point |
| 19i |
Expansion volume |
1 floating point |
| 19j |
Expansion volume deviation |
1 floating point |