Atomic Weights and Cross-Sectional Areas
Atomic Weights and Cross-sectional Areas for Selected Metals
| Metal |
Symbol |
Atomic Weight (g/mol) |
Cross-sectional Area (nm2) |
Density (g/mL) |
| chromium |
Cr |
51.996 |
0.0635 |
7.19 |
| cobalt |
Co |
58.933 |
0.0662 |
8.9 |
| copper |
Cu |
63.54 |
0.0680 |
8.96 |
| gold |
Au |
196.967 |
0.08696 |
18.9 |
| hafnium |
Hf |
178.490 |
0.0862 |
13.3 |
| iridium |
Ir |
192.220 |
0.0769 |
22.4 |
| iron |
Fe |
55.847 |
0.0613 |
7.89 |
| manganese |
Mn |
54.938 |
0.0714 |
7.43 |
| molybdnum |
Mo |
95.940 |
0.0730 |
10.22 |
| nickel |
Ni |
58.710 |
0.0649 |
8.9 |
| niobium |
Nb |
92.906 |
0.0806 |
8.57 |
| osmium |
Os |
190.220 |
0.0629 |
22.6 |
| palladium |
Pd |
106.400 |
0.0787 |
12.02 |
| platinum |
Pt |
195.090 |
0.0800 |
21.45 |
| rhenium |
Re |
186.2 |
0.0649 |
21.02 |
| rhodium |
Rh |
102.905 |
0.0752 |
12.1 |
| tuthenium |
Ru |
101.070 |
0.0613 |
12.4 |
| silver |
Ag |
107.868 |
0.0869 |
10.5 |
| tantalum |
Ta |
180.947 |
0.0800 |
16.6 |
| thorium |
Th |
232.038 |
0.1350 |
11.7 |
| tin |
Sn |
118.710 |
0.1082 |
4.54 |
| tungsten |
W |
183.850 |
0.0741 |
19.3 |
| vanadium |
V |
50.942 |
0.0680 |
6.11 |
| zirconium |
Zr |
91.220 |
0.0877 |
6.51 |
Copyright © 2022 - 2024. Micromeritics Instrument Corporation. All rights reserved.