Active Metals for Chemisorption Analyzers

Or, click Active Metals on the Sample Description tab when using the Advanced presentation option.

Atomic Weights and Cross-Sectional Areas

Up to 20 elements can be specified. At least one element must have a non-zero % of the sample weight.

Active Metals
Selections Description
Atomic Cross Sect.
Area (nm2) [column]
Atomic cross-sectional area of the element.
Atomic Weight [column] Atomic weight of the element.
Density g/cm3 [column] Density of the element.
Element [drop‑down box] Select or enter the active metal.
  For fields and buttons not listed in this table, see Common Fields and Buttons.