Theory
Mercury porosimetry is based on the capillary law governing liquid penetration into small pores. This law, in the case of a non-wetting liquid like mercury and cylindrical pores, is expressed by the Washburn equation
where D is pore diameter, P the applied pressure, γ the surface tension, and ϕ the contact angle, all in consistent units. The volume of mercury V penetrating the pores is measured directly as a function of applied pressure. This P-V information serves as a unique characterization of pore structure.
Pores are rarely cylindrical, hence the above equation constitutes a special model. Such a model may not best represent pores in actual materials, but its use is generally accepted as the practical means for treating what, otherwise, would be a most complex problem.
The surface tension of mercury varies with purity; its usually accepted value and the value recommended here is 485 dynes/cm. The contact angle between mercury and the solid containing the pores varies somewhat with solid composition. A value of 130 degrees is recommended in the absence of specific information to the contrary.
Mercury extruding from pores upon reduction of pressure is in general accord with the above equation, but indicated pore diameters are always offset toward larger diameters. This results from equivalent volumes of mercury extruding at pressures lower than those at which the pores were intruded. It is also commonly observed that actual pores always trap mercury. The first phenomena is usually attributed to receding contact angles being less than advancing ones. The second is likely due to pore irregularities giving rise to enlarged chambers and “inkwell” structures. These phenomena give rise to hysteresis phenomena, i.e., distinct intrusion and extrusion P-V curves.