Graph Report Options
- Cumulative Area vs Size Plot Options
- Cumulative Volume vs Pressure Plot Options
- Cumulative Volume vs Size Plot Options
- Difference from Reference % Volume Plot Options
- Differential Intrusion Plot Options
- Differential Volume vs Size Plot Options
- Incremental Volume vs Pressure Plot Options
- Incremental Volume vs Size Plot Options
- Log Differential Intrusion Plot Options
- Out of Specification % Volume Plot Options
| Field or Button | Description | ||
|---|---|---|---|
| Autoscale [check box] | When enabled on the report parameters windows, allows the x- and y‑ axes to be scaled automatically. Autoscale means that the x‑ and y‑ ranges will be set so that all the data is shown. If Autoscale is not selected, the entered range is used. | ||
| Options [check box] |
Plot Points. Select to plot the points on the graph. Plot Curve. Interpolated from data points. Show As Histogram. When selected, Plot Points and Plot Curve options are disabled. |
||
| Overlays [button] | Select sample files that contain data to be overlayed onto the selected plot. | ||
| Reference [button] | Select a sample file to compare analysis results of the current sample. | ||
| Specification [button] | Specify sample files to use for the boundaries of the coarse and fine specifications. | ||
| X-Axis [group box] |
Select options for the x-axis. Variable. Scale. |
||
| Y-Axis [group box] |
Select options for the y-axis. Variable. Select the y-axis variable from the drop-down list. Overlay. [Optional]. Select an option to overlay. Intrusion / Extrusion. Select the data points to plot.
|
||
|
|||