PSD History Report
Reports > PSD History
The PSD History Report generates a sequence of full pore size distribution graphs.
| Field or Button | Description | ||
|---|---|---|---|
| Report [button] | Generates the report. | ||
| Samples [button] | Select additional sample files to add to the report. | ||
| Save as Default [button] | Click to save selected report options as default report settings. | ||
| Show [selection] |
Select one of the following options: First Intrusion. Select to show the first intrusion segment. First Extrusion. Select to show the first extrusion segment. |
||
| Show bitmap [check box] |
Use to show a graphic on the report header. Height / Width. Enter the height and width of the selected graphic. These values determine the graphic appearance on the generated report. |
||
| Show report title [check box] |
Select and enter a report title to appear on the report header. | ||
| X-axis Order By [selection] |
Select one of the following: Time. Time the files were analyzed. File name. Alphanumeric order. |
||
| X Axis variable [selection] |
Select one of the following to display on the graph: Pressure. Pore size. |
||
| Y Axis variable [selection] |
Select one of the following to display on the graph: Diff. volume. Diff. % volume. Diff. area. |
||
|
|||