Formula Correction
A formula for correction is available for each type of penetrometer. The formula is a part of the application software, therefore when the Formula option in the Penetrometer Properties file is selected, the formula is applied.
The recommended method of correction is by blank correction file. The formula is provided for use when comparison with historical data is required.