Sample Averaging
File > Average
A sample file can be created in which the collected data are the average of up to four similar analyses. All information in the new sample file will be the same as in the first selected file except for the information entered in the Sample Averaging window. The collected data in the file will be the average of the data in the selected files.
Sample averaging can be used for sample files and blank correction files.