MicroActive for AutoPore V 9600
v2.03

Allow data selection by particle size range.

-----------------------------------------------------------------------------
v2.02

Improvement to high pressure checks.

-----------------------------------------------------------------------------
v2.01

Improvements to tabular reports.

-----------------------------------------------------------------------------
v2.00

Add support for the 9600 and 9610.

-----------------------------------------------------------------------------
v1.03

1. Improvements in the control of the high pressure pump.  
2. Improvements to sample based blank correction.  
3. Improvements in peak table report. 

-----------------------------------------------------------------------------
V1.02

1. Allow the pore structure report to optionally use the calculated total 
   pore area.
2. Fix issues with overlays and with selected pressure ranges in reports.

-----------------------------------------------------------------------------
V1.01

1. Allow pressure ranges to be specified per report.
2. Add Mayer-Stowe and pore structure as individual reports in addition to 
   their optional inclusion in the summary report.

-----------------------------------------------------------------------------
V1.00

Initial release of this product.